Acrílico (PMMA) is a popular material in Usinagem CNC for its transparency and ease of shaping—but getting the speed of acrylic for CNC machining right is make-or-break. Muito lento, e você perde tempo; muito rápido, e você corre o risco de quebrar a ferramenta, mau acabamento superficial, ou até mesmo acrílico derretido. This guide breaks down how to set optimal speeds for different tools, fix common speed-related issues, and achieve consistent, resultados de alta qualidade.
1. Key Factors That Determine CNC Acrylic Machining Speed
Before setting speeds, you need to understand the variables that influence performance. Ignore these, and even “standard” speeds will fail:
| Fator | How It Affects Speed | Example Impact |
|---|---|---|
| Tipo de ferramenta & Contagem de dentes | Drill bits vs. milling cutters have different speed limits; more teeth = more heat (needs slower speeds) | A 6-tooth drill bit can’t handle 24,000 RPM (like a 2-tooth one)—it’ll overheat and dull |
| Diâmetro da ferramenta | Smaller tools = higher max speed; larger tools = lower max speed | A 3.175mm drill bit hits 24,000 RPM, but a 10mm drill bit tops out at 15,000 RPM |
| Acrylic Thickness | Thicker acrylic = slower feed speed (para evitar rachaduras); thinner acrylic = faster feed speed | Machining 10mm thick acrylic needs a feed speed of 50–80 mm/min; 3mm thick can use 100–120 mm/min |
| Machine Performance | Low-power machines (≤1.5kW) can’t reach high RPM; high-power machines (≥3kW) handle faster speeds | A 1.5kW CNC router maxes out at 18,000 RPM for drills; a 3kW machine hits 24,000 RPM |
Por que isso importa? Using a 4-tooth drill bit at 24,000 RPM (the speed for a 2-tooth one) creates excess friction—within 5 minutos, the tool will overheat, lose sharpness, and leave rough edges on the acrylic.
2. Optimal Speed Settings for Common CNC Tools
The right speed depends on whether you’re using a drill bit or a milling cutter. Below are tested, practical speed ranges (with examples) to avoid mistakes:
2.1 Drill Bit Speed: By Tooth Count & Diâmetro
Drill bits are for making holes—and their speed must match tooth count to prevent overheating. The table below is your go-to reference:
| Drill Bit Specs | RPM Range | Cenário de exemplo | Risk of Wrong Speed |
|---|---|---|---|
| 2-dente (twist drill), 3.175milímetros | 8,000–24,000 RPM | Low-speed (8,000 RPM): Thick acrylic (15milímetros); De alta velocidade (24,000 RPM): Thin acrylic (3milímetros) | Muito lento: Takes 2x longer; Muito rápido: Melts acrylic around the hole |
| 4-dente, any diameter | 6,000–15.000 RPM | Drilling a 5mm hole in 8mm acrylic: 10,000 RPM | Sobre 15,000 RPM: Tool dulls in 10 buracos (contra. 50 holes at 10,000 RPM) |
| 6-dente, any diameter | 5,000–12.000 RPM | Drilling a 8mm hole in 10mm acrylic: 8,000 RPM | Sobre 12,000 RPM: Tool may break mid-drill (due to heat stress) |
Para dica: For 4-tooth or 6-tooth drill bits, start at the lower end of the RPM range and increase by 1,000 RPM if the cut is smooth (no melting or vibration).
2.2 Milling Cutter Speed: Velocidade do fuso + Velocidade de alimentação
Milling cutters shape acrylic (por exemplo, bordas, slots) and need a balance of spindle speed (RPM) and feed speed (how fast the tool moves). Here’s how to pair them:
| Milling Cutter Type | Velocidade do fuso (RPM) | Velocidade de alimentação (mm/min) | Ideal Use Case |
|---|---|---|---|
| Fresa final (2-flauta), 6milímetros | 15,000–20.000 RPM | 80–120 mm/min | Trimming the edge of a 100x50mm acrylic sheet |
| Fresa frontal (4-flauta), 12milímetros | 12,000–18,000 RPM | 60–100 mm/min | Flattening the surface of a 200x200mm acrylic block |
Critical Rule: Never let the milling cutter stay in one spot for more than 2 segundos. Pausing creates heat, which melts acrylic and sticks chips to the part—ruining surface finish (you’ll see foggy, rough areas instead of clear edges).
3. How to Troubleshoot Speed-Related CNC Acrylic Machining Issues
Even with the right settings, problems can happen. Use this checklist to fix common speed-related errors:
| Problema | Causa raiz (Speed-Related) | Step-by-Step Solution |
|---|---|---|
| Melted acrylic around cuts | RPM muito alto; feed speed too slow (tool rubs instead of cutting) | 1. Reduce RPM by 2,000–3,000; 2. Increase feed speed by 20 mm/min; 3. Check for tool dullness (replace if needed) |
| Tool breaks mid-machining | RPM muito alto (heat stress); feed speed too fast (excess force) | 1. Lower RPM to the bottom of the recommended range; 2. Slow feed speed by 10–15 mm/min; 3. Ensure acrylic is clamped tightly (vibration worsens stress) |
| Duro, foggy surface finish | RPM too low (tool tears acrylic instead of cutting cleanly) | 1. Increase RPM by 1,000–2,000; 2. Use a fresh tool (dull tools cause roughness); 3. Add a coolant (water-based) para reduzir o atrito |
Exemplo: A user was machining a 5mm thick acrylic sign with a 3.175mm 2-tooth drill bit at 24,000 RPM and 40 mm/min feed speed. The acrylic melted around the holes. Solução: Lower RPM to 18,000 and increase feed speed to 60 mm/min—melting stopped, and holes were clean.
4. Perspectiva da Tecnologia Yigu
Na tecnologia Yigu, we know optimizing the speed of acrylic for CNC machining is key to reducing waste and boosting efficiency. Many clients struggle with balancing speed and quality—our advice is to start with the “middle ground” of recommended RPM ranges (por exemplo, 16,000 RPM for 2-tooth 3.175mm drills) and adjust based on real-time feedback. We’re also integrating speed-presets into our CNC control software for common acrylic jobs (por exemplo, drilling 3mm holes), cutting setup time by 40%. As acrylic use grows in signage and electronics, precise speed control will only become more critical—and we’re here to simplify it for every user.
5. Perguntas frequentes: Answers to Common Speed Questions
1º trimestre: Can I use the same RPM for different acrylic thicknesses?
A1: No—thicker acrylic needs slower RPM. Por exemplo, a 3.175mm 2-tooth drill bit uses 24,000 RPM for 3mm acrylic but 8,000 RPM for 15mm acrylic. Slower speeds prevent overheating in thick material.
2º trimestre: What if my CNC machine can’t reach the recommended RPM?
A2: Compensate with feed speed. If your machine maxes out at 15,000 RPM (em vez de 20,000 for a milling cutter), slow feed speed by 20% (por exemplo, de 100 para 80 mm/min) to reduce tool stress.
3º trimestre: How often should I check speed settings?
A3: Every time you change tools or acrylic thickness. Even a small tool diameter change (por exemplo, 3mm to 5mm) needs a RPM adjustment—skipping this leads to errors.