In CNC machining of aluminum parts—from NEV battery brackets to consumer electronics housings—the rotation speed of CNC machining aluminum directly affects cutting efficiency, vida útil da ferramenta, e qualidade da superfície da peça. Uma velocidade muito alta causa superaquecimento e desgaste da ferramenta; muito baixo leva a baixa produtividade e mau acabamento superficial. Este artigo analisa os principais fatores de influência, calculation methods, typical speed references, parameter coordination strategies, and practical adjustment tips, helping you accurately set and optimize rotation speeds for different aluminum machining scenarios.
1. What Are the Core Factors Influencing Rotation Speed of CNC Machining Aluminum?
The rotation speed isn’t a fixed value—it depends on four interconnected factors. Understanding these helps avoid blind adjustment and ensures stable machining.
| Influencing Factor | Key Details | Impact on Rotation Speed | Practical Example |
| Aluminum Alloy Type | Different alloys have varying hardness and machinability: – 6061 liga de alumínio: Low hardness (HB 60-80), boa usinabilidade – 7075 liga de alumínio: Alta dureza (HB 150-180), alta resistência | 6061 allows 20-30% higher speeds than 7075; Harder alloys require lower speeds to prevent tool overload | For a Φ10mm carbide tool: 6061 usa 3000-4000 RPM; 7075 usa 2200-3000 RPM |
| Tool Type & Material | Tool materials determine speed limits: – Ferramentas de metal duro: Alta resistência ao desgaste, support high speeds – Aço rápido (HSS) ferramentas: Low heat resistance, limited to low speeds – Coated tools (por exemplo, TiAlN): Reduza o atrito, increase speed upper limit by 15-25% | Carbide tools run 2-3x faster than HSS; Coated carbide outperforms uncoated by 15-25% | Φ10mm tool for 6061 alumínio: HSS uses 1200-1800 RPM; Uncoated carbide uses 3000-4000 RPM; TiAlN-coated carbide uses 3500-4800 RPM |
| Tool Diameter | Small-diameter tools have higher rotational inertia and are prone to vibration at low speeds; Large-diameter tools generate more cutting force, requiring lower speeds to avoid machine vibration | Speed is inversely proportional to tool diameter (per the core formula); Small tools (≤Φ5mm) need 2-3x higher speeds than large tools (≥Φ25mm) | Para 6061 aluminum with carbide tools: Φ5mm tool uses 6000-8000 RPM; Φ25mm tool uses 1200-1600 RPM |
| Processing Stage | Roughing prioritizes material removal; Finishing focuses on surface quality: – Roughing: Larger cutting depth (1-3milímetros), needs medium speed to balance efficiency and tool load – Acabamento: Smaller cutting depth (0.1-0.5milímetros), requires higher speed for smooth surfaces | Finishing speeds are 30-50% higher than roughing speeds for the same tool and alloy | Φ10mm carbide tool on 6061 alumínio: Roughing uses 3000-3500 RPM; Finishing uses 4000-4800 RPM |
2. How to Calculate Rotation Speed of CNC Machining Aluminum?
The rotation speed is calculated using a universal formula, with cutting speed (Vc) as the core reference. Mastering this formula allows you to derive speeds for different tool and alloy combinations.
2.1 Core Calculation Formula
The standard formula for rotation speed (RPM) é:
RPM = (Cutting Speed (Vc) × 1000) / (π × Tool Diameter (D))
- Vc (Cutting Speed): The linear speed of the tool’s cutting edge relative to the workpiece (unidade: m/meu), determined by alloy type and tool material.
- D (Tool Diameter): The outer diameter of the cutting tool (unidade: milímetros).
- π: A constant (≈3.1416).
2.2 Step-by-Step Calculation Example
Let’s calculate the rotation speed for machining 6061 aluminum with a Φ10mm TiAlN-coated carbide tool:
- Determine Vc: For TiAlN-coated carbide tools machining 6061 alumínio, the recommended Vc is 100-130 m/meu (padrão da indústria).
- Plug into the formula:
- If Vc = 100 m/meu: RPM = (100 × 1000) / (3.1416 × 10) ≈ 3183 RPM
- If Vc = 130 m/meu: RPM = (130 × 1000) / (3.1416 × 10) ≈ 4138 RPM
- Final Speed Range: 3183-4138 RPM (rounded to 3200-4100 RPM for practical use).
2.3 Cutting Speed (Vc) Reference for Common Scenarios
To simplify calculation, below is a Vc reference table for different aluminum alloys and tool materials:
| Liga de alumínio | Tool Material | Recommended Vc Range (m/meu) | Applicable Processing Stage |
| 6061 (Low Hardness) | HSS | 30-50 | Roughing (produção de baixo volume) |
| 6061 | Uncoated Carbide | 80-110 | Roughing (produção em massa) |
| 6061 | TiAlN-Coated Carbide | 100-130 | Acabamento (high surface quality needs) |
| 7075 (Alta Dureza) | Uncoated Carbide | 60-80 | Roughing (avoid tool overload) |
| 7075 | TiAlN-Coated Carbide | 75-100 | Acabamento (balance speed and tool life) |
3. What Are the Typical Rotation Speed References for CNC Machining Aluminum?
Based on tool diameter, alloy type, and processing stage, we’ve summarized practical speed ranges for common scenarios—saving you time on repeated calculations.
3.1 Rotation Speed by Tool Diameter (para 6061 Alumínio, Ferramentas de metal duro)
| Tool Diameter (D) | Roughing Rotation Speed (RPM) | Finishing Rotation Speed (RPM) | Key Application |
| Φ3-5mm (Pequeno) | 4500-6000 | 6000-8000 | Fine features: Sensor mounting holes, thin-wall grooving |
| Φ8-12mm (Médio) | 2800-3500 | 3500-4800 | General machining: Housing outer contours, boss milling |
| Φ15-20mm (Grande) | 1800-2500 | 2500-3200 | Large-area roughing: Battery tray bottom surfaces |
| Φ25mm+ (Extra-Large) | 1200-1800 | 1800-2200 | Heavy cutting: Thick aluminum plate material removal |
3.2 Speed Adjustment for 7075 Alumínio (contra. 6061)
Desde 7075 is harder, reduce the speed by 20-30% comparado com 6061 for the same tool and processing stage. Exemplo:
- Φ10mm TiAlN-coated carbide tool: 6061 finishing uses 3500-4800 RPM; 7075 finishing uses 2500-3500 RPM.
4. How to Coordinate Rotation Speed with Other Key Parameters?
Rotation speed doesn’t work in isolation—it must be matched with feed speed, cutting depth, and cooling to avoid defects. Below is a coordinated parameter guide:
4.1 Feed Speed Coordination
Feed speed (F) is calculated as: F = RPM × Number of Tool Teeth (Z) × Feed per Tooth (fz). For aluminum, fz ranges from 0.1-0.3mm/tooth (adjust based on speed).
| Rotation Speed (RPM) | Number of Tool Teeth (Z) | Feed per Tooth (fz, mm/tooth) | Recommended Feed Speed (F, mm/min) |
| 3000 (Medium Speed) | 4 | 0.2 | 3000×4×0.2 = 2400 |
| 6000 (High Speed) | 2 (Small-diameter tool) | 0.12 | 6000×2×0.12 = 1440 |
| 1500 (Low Speed) | 6 (Large-diameter tool) | 0.25 | 1500×6×0.25 = 2250 |
Critical Note: High speed + high feed speed causes tool overheating—reduce fz by 10-20% when RPM exceeds 5000.
4.2 Cutting Depth Matching
Cutting depth (ap) affects tool load—deeper cuts require lower speeds to prevent tool deflection.
| Processing Stage | Cutting Depth (ap, milímetros) | Recommended Rotation Speed Adjustment |
| Roughing | 1-3 | Use the lower end of the speed range (por exemplo, 2800-3200 RPM for Φ10mm tool) |
| Semi-Finishing | 0.5-1 | Use the middle of the speed range (por exemplo, 3200-3800 RPM for Φ10mm tool) |
| Acabamento | 0.1-0.5 | Use the upper end of the speed range (por exemplo, 3800-4800 RPM for Φ10mm tool) |
4.3 Resfriamento & Lubrication Support
Effective cooling allows higher speeds by reducing cutting temperature (aluminum melts at ~660°C—overheating causes tool adhesion).
| Cooling Method | Speed Increase Potential | Application Scenario |
| Water-Based Coolant (Concentration 5-8%) | 15-20% | Produção em massa (por exemplo, NEV part machining lines) |
| Oil-Based Coolant | 10-15% | High-precision finishing (avoids corrosion on aluminum) |
| Micro-Lubrication (Air-Oil Mist) | 5-10% | Dry workshops or small-batch machining |
5. What Are the Practical Tips for Adjusting Rotation Speed?
Even with theoretical references, on-site adjustment is needed to adapt to equipment and workpiece variations. Below are 4 actionable tips:
- Start with Conservative Speeds
For new alloy-tool combinations, set RPM to 80% of the recommended upper limit. Por exemplo, if the theoretical range is 3000-4000 RPM, start at 3200 RPM. Observe chip shape (ideal chips: continuous, curled, silver-white) and machine sound (no high-pitched squealing or vibration) to avoid initial tool damage.
- Check Dynamic Balance for High-Speed Machining
When RPM exceeds 5000, use a dynamic balance tester to adjust tool holders (balance grade G2.5 or higher). Unbalanced tools cause vibration, reducing surface quality (Ra increases from 0.8μm to 3.2μm) and shortening tool life by 30-50%.
- Adjust Based on Spindle Type
Spindle rigidity limits maximum speed:
- BT30 spindles (small machines): Max stable speed ≤8000 RPM (avoid overloading).
- BT40 spindles (medium machines): Max stable speed ≤12000 RPM (suitable for high-speed finishing).
- Use CAM Software for Simulation
Tools like Mastercam or UG can simulate cutting forces and temperatures at different speeds. Para peças complexas (por exemplo, thin-walled aluminum housings), simulation helps identify speed-related risks (por exemplo, vibration at corners) and optimize parameters in advance—reducing trial-and-error time by 40-60%.
6. Yigu Technology’s Perspective on Rotation Speed of CNC Machining Aluminum
Na tecnologia Yigu, we see the rotation speed of CNC machining aluminum as the “balance point of efficiency and quality”—it’s not about pursuing the highest speed, but matching speed to actual production needs. Our data shows 60% of aluminum machining defects (desgaste da ferramenta, mau acabamento superficial) come from mismatched speeds, not equipment issues.
We recommend a “scenario-driven” adjustment approach: Para 6061 aluminum NEV battery brackets (produção em massa), we use TiAlN-coated carbide tools + water-based coolant, setting RPM to 3500-4000 RPM to balance efficiency and tool life; Para 7075 aluminum aerospace parts (alta precisão), we lower RPM to 2500-3000 RPM and reduce feed per tooth to 0.15mm/tooth, ensuring surface Ra ≤0.8μm. We also integrate real-time temperature sensors to monitor tool conditions, auto-adjusting speed by 5-10% if overheating is detected—helping clients reduce tool costs by 20% and improve production efficiency by 15%.
7. Perguntas frequentes: Common Questions About Rotation Speed of CNC Machining Aluminum
Q1: Can I use the same rotation speed for both roughing and finishing of the same aluminum part?
Não. Roughing requires medium speed (to handle large cutting depth and avoid tool overload), while finishing needs higher speed (to achieve smooth surfaces). Por exemplo, a Φ10mm carbide tool on 6061 alumínio: Roughing uses 3000-3500 RPM, finishing uses 3800-4800 RPM. Using the same speed leads to either low roughing efficiency or excessive finishing tool wear.
Q2: Why does a small-diameter tool (por exemplo, Φ5mm) need a much higher rotation speed than a large-diameter tool (por exemplo, Φ25mm)?
It’s due to cutting speed (Vc) consistência. Per the formula RPM = (Vc×1000)/(π×D), smaller D requires higher RPM to maintain the same Vc (critical for cutting efficiency). Para 6061 aluminum with Vc=100 m/min: Φ5mm tool needs ~6366 RPM, Φ25mm tool needs ~1273 RPM. A low speed for small tools would result in low Vc, leading to slow material removal and poor surface finish.
Q3: How to handle rotation speed adjustment when machining thin-walled aluminum parts (thickness ≤2mm)?
Thin-walled parts are prone to vibration—use these strategies: 1. Increase RPM by 10-15% (por exemplo, de 3500 para 4000 RPM for Φ10mm tool) to reduce cutting force; 2. Reduce feed per tooth by 20-30% (de 0.2 to 0.14mm/tooth) to avoid part deformation; 3. Use micro-lubrication to minimize heat-induced warping. These steps balance speed and part stability.