A usinagem CNC depende de três elementos principais para fornecer eficiência, resultados de alta qualidade: velocidade de corte, avanço da ferramenta, e depth of cut. Esses elementos são como o “motor, transmissão, e combustível” de um carro – cada um funciona de forma independente, mas deve ser equilibrado para evitar erros como danos à ferramenta, mau acabamento superficial, ou tempo perdido. Este guia detalha cada element of CNC machining, solves common parameter-setting problems, and helps you optimize them for your specific project.
1. Cutting Speed: The “Speed Limit” for Tool and Material
Cutting speed is the speed at which the workpiece or tool moves relative to each other during machining (measured in m/min or ft/min). It directly impacts how fast you can machine a part—and how long your tool lasts.
1.1 Key Factors That Determine Cutting Speed
Cutting speed isn’t one-size-fits-all. It depends on three critical factors:
- Tool Material: Harder tools handle faster speeds. Ferramentas de metal duro (common in industrial CNC) can run 3–5x faster than high-speed steel (HSS) ferramentas.
- Workpiece Material: Materiais macios (por exemplo, alumínio) allow faster speeds than hard materials (por exemplo, aço inoxidável).
- Machining Conditions: Wet machining (with coolant) lets you increase speed by 20–30% (coolant reduces heat and tool wear).
The table below shows recommended cutting speeds for common tool-workpiece pairs:
| Tool Material | Workpiece Material | Dry Machining Speed (m/meu) | Wet Machining Speed (m/meu) |
| Carboneto | Alumínio | 300–500 | 400–600 |
| Carboneto | Aço inoxidável | 80–120 | 100–150 |
| HSS | Alumínio | 100–150 | 120–180 |
| HSS | Aço inoxidável | 20–40 | 30–50 |
1.2 Common Problem Solved: “Why is my tool wearing out too fast?”
You’re likely using a cutting speed that’s too high for your tool-workpiece pair. Por exemplo:
- If you run a carbide tool on stainless steel at 200 m/meu (seco), the tool will overheat and wear out in 30 minutos.
- Lower the speed to 100 m/meu (seco), and the tool lasts 4–6 hours—saving you money on tool replacements.
2. Tool Feed: Balancing Surface Quality and Efficiency
Tool feed is the distance the tool moves along the workpiece per revolution (measured in mm/rev or inches/rev). It controls two key outcomes: rugosidade superficial (how smooth the part is) and machining time.
2.1 How to Choose Tool Feed
The right feed rate depends on whether you’re doing rough machining (removing material quickly) ou finish machining (creating a smooth surface):
- Usinagem Desbaste: Use a larger feed rate (0.2–0.5 mm/rev) to remove material fast. Por exemplo, when cutting a 100mm aluminum block down to 80mm, um 0.4 mm/rev feed cuts the block in 5 minutos (contra. 10 minutes with a 0.2 mm/rev feed).
- Acabamento de usinagem: Use a smaller feed rate (0.05–0.15 mm/rev) para superfícies lisas. UM 0.1 mm/rev feed on a stainless steel part creates a surface roughness (Rá) de 1.6 μm—smooth enough for visible parts like consumer electronics.
2.2 Critical Considerations
- Machine Power: A weak CNC machine (low horsepower) can’t handle large feed rates—too much feed will stall the spindle.
- Tool Rigidity: Longo, thin tools need smaller feeds (0.05–0.1 mm/rev) to avoid vibration (which ruins surface quality). Curto, thick tools can handle larger feeds.
Exemplo: A user is finish-machining a aluminum phone case. They start with a 0.2 mm/rev feed and get a rough surface (Rá 6.3 μm). They lower the feed to 0.1 mm/rev, and the surface becomes smooth (Rá 1.6 μm)—perfect for a consumer product.
3. Depth of Cut: Minimizing Passes Without Breaking Tools
Depth of cut is the distance the tool penetrates into the workpiece per pass (measured in mm or inches). It’s all about efficiency—using a larger depth reduces the number of passes, but too much depth can damage the tool or workpiece.
3.1 Rules for Choosing Depth of Cut
Follow these guidelines to avoid mistakes:
- Prioritize Large Depths (When Possible): On rough machining, use the largest depth your tool and machine can handle. For a carbide tool cutting aluminum, a 5–10 mm depth per pass is safe—this cuts a 50mm thick block in 5–10 passes (contra. 25 passes with a 2 mm profundidade).
- Limit Depth for Hard Materials: For stainless steel or titanium, keep depth under 2–3 mm per pass (hard materials put more stress on tools).
- Finish Machining Needs Small Depths: Use a 0.1–0.5 mm depth for finish passes—this removes small imperfections without altering the part’s dimensions.
3.2 Common Problem Solved: “Why is my workpiece deforming during machining?”
You’re using a depth of cut that’s too large for the workpiece’s rigidity. Por exemplo:
- A thin aluminum sheet (2mm de espessura) can’t handle a 1.5 mm depth of cut—the sheet will bend under the tool’s force.
- Reduce the depth to 0.5 mm per pass, and the sheet stays flat—ensuring the final part meets your size requirements.
4. How to Balance the Three Elements: Um guia passo a passo
The biggest challenge isn’t setting each element individually—it’s balancing them to get fast, resultados de alta qualidade. Follow this process:
- Start with Cutting Speed: Pick a speed based on your tool and workpiece (use the table in Section 1.1). Por exemplo: Carbide tool + aluminum = 400 m/meu (wet).
- Choose Tool Feed: Match feed to machining type. Rough machining = 0.3 mm/rev; finish machining = 0.1 mm/rev.
- Set Depth of Cut: Use the largest safe depth. For rough machining: 8 mm per pass (alumínio); for finish machining: 0.3 mm per pass.
- Test and Adjust: Run a small test part. If the tool wears fast, lower the speed. If the surface is rough, reduce the feed. If the part deforms, decrease the depth.
Exemplo: A manufacturer needs to machine 100 suportes de alumínio. They balance the elements as follows:
- Cutting Speed: 400 m/meu (carboneto + wet machining).
- Tool Feed: 0.3 mm/rev (duro) → 0.1 mm/rev (terminar).
- Depth of Cut: 8 milímetros (duro) → 0.3 milímetros (terminar).
Resultado: Each bracket takes 12 minutes to make (contra. 20 minutes with unbalanced settings), and the tools last 8 horas.
5. Real-World Scenarios: Applying the Elements to Common Projects
See how the three elements work together for different CNC jobs:
| Project | Tool/Workpiece | Cutting Speed (m/meu) | Tool Feed (mm/rev) | Depth of Cut (milímetros) | Machining Time per Part |
| Aluminum Phone Case | Carbide/Aluminum | 400 (wet) | 0.3 (duro) → 0.1 (terminar) | 5 (duro) → 0.3 (terminar) | 12 minutos |
| Stainless Steel Gear | Carbide/Stainless Steel | 120 (wet) | 0.2 (duro) → 0.08 (terminar) | 2 (duro) → 0.2 (terminar) | 45 minutos |
| HSS Drill Bit (HSS/Steel) | HSS/Carbon Steel | 30 (seco) | 0.15 (perfuração) | 10 (single pass) | 8 minutos |
Yigu Technology’s Perspective
Na tecnologia Yigu, we know mastering the elements of CNC machining is key to solving users’ efficiency and quality pain points. Many clients struggle with unbalanced parameters—wasting time on slow speeds or replacing tools too often. Our solutions include a “Parameter Matching Tool” that recommends cutting speed, feed, and depth based on tool/workpiece pairs. We also offer carbide tool bundles optimized for common materials (por exemplo, aluminum-specific carbide tools) to simplify setup. As CNC tech evolves, we’ll add AI-powered sensors to auto-adjust elements in real time, helping users achieve precision without manual trial-and-error.
Perguntas frequentes
1. Can I use the same cutting speed for all machining operations (fresagem, perfuração, girando)?
No—operations have different requirements. Drilling needs slower speeds than milling (drills have smaller cutting edges that overheat faster). Por exemplo: Carbide drill on aluminum = 250 m/meu (contra. 400 m/min for milling with the same tool).
2. What happens if I set the tool feed too low?
A too-low feed rate wastes time (por exemplo, um 0.05 mm/rev feed on rough machining doubles the time) and can cause “rubbing” (the tool slides over the workpiece instead of cutting), which wears out the tool faster. Aim for the largest feed rate that keeps surface quality or efficiency on track.
3. Do I need to adjust depth of cut for different tool types?
Sim! Fresas finais (used for milling) can handle larger depths than drills (used for holes). A 10mm end mill on aluminum can take an 8mm depth, but a 10mm drill should only take 2–3mm per pass (drills are less rigid and prone to breaking with large depths).