If you’re a product engineer or procurement professional working on prototypes, Anda tahu betapa kritikalnyaCNC machining PC prototype parts is for turning design ideas into tangible, Komponen berkualiti tinggi. Polikarbonat (Pc) stands out as a top choice for prototypes thanks to its unbeatable mix of strength, ketelusan, and thermal stability. But to get the best results, you need a clear grasp of the entire process—from design to quality checks. Panduan ini memecah setiap langkah, Saham contoh dunia sebenar, and gives data-driven tips to help you avoid mistakes and cut costs.
1. Why Choose PC Material for CNC Machined Prototypes?
Sebelum menyelam ke dalam proses, let’s first understand whyPc (polikarbonat) is a go-to for prototype parts. Unlike other plastics like acrylic or ABS, PC offers a rare combination of properties that solve common prototype challenges:
- Kekuatan impak yang tinggi: PC can withstand 250x more impact than glass and 30x more than acrylic. This is a game-changer for prototypes that need to test durability—like a medical device housing or a consumer electronics cover.
- Ketelusan: Dengan 90% penghantaran cahaya (similar to glass), PC is perfect for prototypes that require see-through parts, such as lens prototypes or dashboard components.
- Kestabilan terma: It can handle temperatures from -40°C to 135°C, making it suitable for prototypes used in harsh environments (Mis., automotive under-hood parts).
Kes sebenar: A startup developing a smart home thermostat needed a transparent prototype cover to showcase its display. By choosing CNC-machined PC instead of acrylic, they avoided cracking during drop tests and ensured the cover stayed clear even when exposed to sunlight for weeks.
2. Langkah 1: 3Reka bentuk d & CNC Programming – The Foundation of Precision
Langkah pertama masukCNC machining PC prototype parts is turning your product idea into a digital plan. This stage directly impacts how accurate and efficient the rest of the process will be.
Tindakan utama:
- Create a 3D Digital Model: Use design software like SolidWorks or AutoCAD to build a detailed 3D model based on your product’s specs (Mis., dimensi, toleransi, dan kemasan permukaan). Contohnya, if you’re making a PC prototype for a drone propeller guard, the model must include exact hole positions and edge curves.
- Menjana kod CNC: Use Computer-Aided Manufacturing (Cam) perisian (such as Mastercam or Fusion 360) to convert the 3D model into G-code- Mesin CNC bahasa memahami. The software optimizes the toolpath to minimize waste and ensure precision.
Critical Tip for Engineers:
Always add clear tolerance labels (Mis., ±0.05mm for critical holes) to your 3D model. A study by the American Society of Mechanical Engineers (Asme) found that 30% of prototype reworks happen because of unclear tolerance instructions.
3. Langkah 2: Material Preparation – Choose the Right PC Stock & Inspect for Defects
Once your design is ready, it’s time to select and prepare thePC material for machining. The quality of your starting material will make or break your prototype.
How to Select PC Stock:
PC is available in sheets, blocks, or rods. The choice depends on your prototype’s size and shape:
Jenis prototaip | Recommended PC Stock Form | Typical Size Range |
---|---|---|
Small covers/lenses | Sheet | 1mm – 20mm thickness |
Large housings | Block | 50mm x 50mm – 300mm x 300mm |
Cylindrical parts (Mis., Tombol) | Rod | 5mm – 100mm diameter |
Defect Inspection:
PC’s high strength means any hidden defects (like air bubbles or scratches) will cause problems during machining (Mis., cracking or uneven cutting). Use these checks:
- Pemeriksaan visual: Look for discoloration or bubbles in the stock.
- Thickness Check: Use a caliper to ensure the stock’s thickness matches your design (toleransi: ± 0.1mm).
Procurement Note: Buy PC stock from certified suppliers (Mis., Sabic or Covestro) to avoid low-quality material. A procurement team at a robotics company once saved $5,000 by rejecting a batch of PC sheets with hidden bubbles—this prevented costly rework later.
4. Langkah 3: CNC Machining PC Parts – Tools, Parameter & Pemantauan
This is the “hands-on” stage where the CNC machine turns the PC stock into your prototype. Machining PC requires specific tools and settings because of its high hardness and strength.
Alat penting & Parameter pemotongan:
Using the wrong tools will lead to rough surfaces or tool wear. Here’s what works best for PC:
Jenis Alat | Bahan | Kelajuan pemotongan (m/my) | Kadar suapan (mm/rev) | Coolant Type |
---|---|---|---|---|
End Mill | Karbida | 150 - 200 | 0.1 - 0.2 | Compressed Air |
Drill Bit | Keluli berkelajuan tinggi (HSS) | 80 - 120 | 0.05 - 0.1 | Water-Soluble Coolant |
What Happens During Machining:
- Set Up the Machine: Secure the PC stock to the CNC table using clamps (avoid over-tightening—this can warp the material).
- Load the Program: Upload the G-code from your CAM software.
- Start Machining: The machine automatically performs memotong, penggilingan, and drilling based on the toolpath.
- Monitor Closely: Operators should check the process every 10 minit. Contohnya, if you’re machining a PC prototype for a baby bottle nipple, you’ll need to ensure the hole for the nipple is drilled straight—even a 0.1mm 偏差 (deviation) can affect functionality.
Contoh sebenar: A medical device company machining PC syringe prototypes used a carbide end mill at 180 m/min and 0.15 mm/rev feed rate. This gave them a smooth surface finish (Ra 0.8 μm) and reduced tool changes by 50% compared to using HSS tools.
5. Langkah 4: Post-Finish Processing – Make Your PC Prototype Perfect
Selepas pemesinan, your PC prototype will have small flaws (like burrs or rough edges) that need fixing. This step is especially important for transparent or high-precision parts.
Common Post-Finish Steps:
- Deburring: Use a sanding pad (120-grit) to remove small burrs from edges. For hard-to-reach areas (Mis., lubang kecil), use a deburring tool.
- Pengamplasan: For non-transparent parts, sand with 240-grit then 400-grit sandpaper to smooth the surface.
- Menggilap (for Transparent Parts): Use a polishing compound (Mis., Cerium oxide) and a buffing wheel to boost clarity. This step can increase light transmission by 5% – critical for lens prototypes.
Petua: Avoid using harsh chemicals (like acetone) on PC—they can damage the material’s surface.
6. Langkah 5: Quality Inspection – Ensure Your Prototype Meets Standards
The final step is to test yourCNC-machined PC prototype to make sure it matches your design. Skipping this step can lead to failed assembly or functional tests later.
Key Inspection Tests:
Jenis ujian | Kaedah | Acceptance Criteria |
---|---|---|
Ketepatan dimensi | Menyelaras mesin pengukur (Cmm) | ±0.03mm for critical dimensions |
Kualiti permukaan | Visual Check + Profilometer | No scratches; Ra ≤ 0.8 μm |
Mechanical Property | Impact Test (Per ASTM D256) | No cracking after 10J impact |
Ketelusan (jika diperlukan) | Light Transmission Meter | ≥85% light transmission |
Kenapa ini penting: A consumer electronics company once skipped the impact test for a PC headphone prototype. When they tested the prototype, it cracked during a drop—delaying their launch by 3 minggu dan kos $10,000 dalam kerja semula.
Yigu Technology’s Perspective on CNC Machining PC Prototypes
Di Yigu Technology, Kami telah menyokong 500 product teams withCNC machining PC prototype parts over the past 8 tahun. We’ve found that the biggest challenge for clients is balancing precision and cost—many teams overspecify tolerances, leading to higher costs. Our solution is to work closely with engineers to optimize designs (Mis., simplifying complex curves) and use high-quality carbide tools to reduce machining time. For transparent PC parts, our specialized polishing process ensures 90% penghantaran cahaya, which is perfect for medical and electronics prototypes. We believe that a collaborative approach—combining your design expertise with our machining experience—is the key to delivering prototypes that meet both functional and budget needs.
FAQ About CNC Machining PC Prototype Parts
- Q: How long does it take to CNC machine a PC prototype part?
A: Ia bergantung pada kerumitan bahagian. A simple PC cover (100mm x 100mm) mengambil masa 1-2 jam, while a complex part (Mis., a PC gear with multiple holes) mengambil masa 4-6 jam. Adding post-finish steps (seperti menggilap) can add 1–3 hours. - Q: Is PC more expensive than other plastics for CNC machining?
A: Ya, PC stock costs about 30% more than ABS, but it’s worth it for prototypes that need strength or transparency. Contohnya, a 100mm x 100mm x 5mm PC sheet costs $15–$20, while an ABS sheet of the same size costs $10–$12. - Q: Can CNC machining PC prototypes achieve tight tolerances?
A: Sudah tentu. With modern CNC machines and carbide tools, we can achieve tolerances as tight as ±0.01mm for small PC parts. Walau bagaimanapun, we recommend only using tight tolerances for critical features (Mis., hole positions) untuk memastikan kos rendah.