How to Sand CNC Plastic Prototypes: 完全なステップバイステップガイド

If you’re a product designer or engineer working with CNCプラスチックプロトタイプ, you know that even the most precise CNC machining leaves small flaws—like tool marks, slight (bulges), または粗いエッジ. サンディング is the critical step that turns these raw parts into smooth, high-quality prototypes ready for testing, presentation, or post-processing (like painting or coating). このガイドで, we’ll break down exactly how to sand your CNC plastic prototype, from choosing the right tools to avoiding common mistakes, so you get consistent, professional results every time.

What Is CNC Plastic Prototype Sanding, and Why Does It Matter?

初め, let’s clarify what sanding does for your CNCプラスチックプロトタイプ. Sanding uses abrasive materials (like sandpaper) to remove surface imperfections, refine shape, and improve smoothness. For CNC plastic parts—made from materials like ABS, PC, or PMMA—this step isn’t just about looks; it directly impacts functionality and 后续 processes (後処理).

Here’s why sanding is non-negotiable for CNC plastic prototypes:

  • Removes machining flaws: CNC tools often leave fine tool marks or “burrs” (tiny plastic bits) on edges. Sanding eliminates these, so the prototype matches your 3D design.
  • Improves surface quality: A smooth surface ensures better adhesion for paint, のり, or coatings. Rough surfaces can cause paint to peel or coatings to bubble.
  • Enhances precision: Light sanding can correct minor size 偏差 (deviations) from CNC machining, ensuring the prototype fits with other parts.
  • Boosts presentation value: A well-sanded prototype looks more professional—critical if you’re sharing it with clients or stakeholders.

Pre-Sanding Preparation: Choose the Right Sandpaper and Tools

Before you start sanding, you need two key things: the right sandpaper grit (abrasiveness level) and suitable sanding tools. Choosing incorrectly can lead to over-sanding (ruining the prototype) or uneven results. Below is a breakdown of what to pick, with data to guide your choice.

1. Sandpaper Grit Selection: From Coarse to Fine

Sandpaper grit is measured by the number of abrasive particles per square inch—the higher the number, the finer the sandpaper. CNCプラスチックプロトタイプ用, you’ll always start with coarse grit and work your way to fine grit. This “progressive sanding” ensures you remove flaws without creating new scratches.

Sandpaper GritType (Application Stage)Surface Roughness After UseProcessing Time per 10cm² Areaに最適です
80–120CoarseInitial sanding10–20 μm1–2分Removing deep tool marks, バリ, または (bulges)
240–400中くらいIntermediate sanding5–10 μm2–3分Smoothing scratches left by coarse grit
600–800FineDetailed sanding2–5 μm3–4 minutesCreating a smooth base for polishing
1000–1200Extra-FinePre-polishing1–2 μm4–5 minutesPreparing surface for mirror-like polishing

ヒントの場合: Never skip a grit level! 例えば, going from 120-grit (coarse) to 600-grit (fine) will leave deep scratches that the fine grit can’t remove—this adds extra time and ruins your finish.

2. Sanding Tool Selection: Manual vs. Electric

The tool you use depends on the prototype’s size, 形, and how much time you have. Manual tools are better for small or detailed parts, while electric tools speed up work on larger prototypes.

ツールタイプ (Suitable Scenarios)効率 (Sanding Speed)長所短所
Manual Sandpaper Sheets小さな部品, タイトコーナー, details遅い (5–10 cm² per minute)低コスト, full control, no risk of over-sandingTime-consuming for large parts
Sanding BlocksFlat or slightly curved surfaces適度 (10–15 cm² per minute)Even pressure, avoids uneven sandingCan’t reach tight gaps or complex curves
Electric Orbital Sander大きな平らな表面 (例えば。, panels)速い (20–30 cm² per minute)Saves time, consistent resultsRisk of over-sanding if used on small parts; needs power
Mini Die Grinder (with sanding bits)Tiny details, 小さな穴適度 (8–12 cm² per minute)Reaches hard-to-access areasRequires skill to avoid damaging the part

Step-by-Step Sanding Process for CNC Plastic Prototypes

Now let’s walk through the sanding process step by step. Follow these steps, and you’ll get a smooth, flawless surface every time—no experience required.

ステップ 1: Initial Sanding (Coarse Grit: 80–120)

The goal here is to remove obvious flaws from CNC machining.

  1. Secure the prototype: Use a clamp or vice to hold the part in place—this keeps it stable and prevents slips (which cause uneven sanding).
  2. Choose your tool: For large flaws (like thick burrs), use a sanding block with 80-grit sandpaper. 小さな部品の場合, use your fingers to hold the sandpaper (wrap it around a flat object for even pressure).
  3. Sand in one direction: Always sand along the plastic’s grain (if it has one) or in a consistent straight line. Circular motions can create swirl marks that are hard to fix later.
  4. Check progress: After 1–2 minutes, wipe the surface with a dry cloth. If tool marks are gone, move to the next grit. そうでない場合, keep sanding—but don’t press too hard (this can warp thin plastic).

ステップ 2: Intermediate Sanding (Medium Grit: 240–400)

This step smooths the scratches left by coarse sandpaper.

  1. Switch to medium grit: Replace your 80–120 grit sandpaper with 240–400 grit.
  2. Lighten pressure: Use half the pressure you used for coarse sanding. Plastic is soft—too much pressure will dig into the surface.
  3. Sand across previous scratches: To erase coarse scratches, sand at a 45° angle to your initial sanding direction. This helps you see when scratches are gone.
  4. Clean the surface: Use a brush to sweep away plastic dust—dust can get trapped in sandpaper and create new scratches.

ステップ 3: Detailed Sanding (Fine Grit: 600–800)

Now you’re refining the surface to make it smooth to the touch.

  1. Use fine-grit sandpaper: 600–800 grit is perfect here. 湾曲した表面用, use a flexible sanding sponge (it conforms to the shape better than a rigid block).
  2. Focus on edges and corners: These areas are easy to miss. Use a small piece of sandpaper folded into a point to reach tight spots (like the inside of a hole).
  3. Check smoothness: Run your finger gently over the surface. If it feels “grainy,” keep sanding for another minute. If it’s smooth, move on.

ステップ 4: Pre-Polishing (Extra-Fine Grit: 1000–1200)

This optional but recommended step prepares the surface for polishing (if you want a mirror finish).

  1. Use extra-fine sandpaper: 1000–1200 grit will make the surface almost smooth enough to polish.
  2. Sand with light, circular motions: 平らな表面用, an electric orbital sander (set to low speed) works best here. 小さな部分の場合, use your fingers with very light pressure.
  3. Wipe with a damp cloth: After sanding, use a damp lint-free cloth to remove all dust. The surface should look uniformly smooth—no visible scratches.

ステップ 5: Final Polishing (Optional: For Mirror Finish)

If you need a glossy, mirror-like surface (例えば。, for a consumer product prototype), add this step.

  1. Gather supplies: You’ll need polishing compound (choose one for plastic, like Meguiar’s PlastX) and a soft cloth or buffing wheel.
  2. Apply polishing compound: Put a small amount (about the size of a pea) on the cloth.
  3. Buff in circular motions: Rub the cloth over the surface with gentle pressure for 2–3 minutes. 大きな部品の場合, use an electric buffing wheel (set to low speed) to save time.
  4. Wipe clean: Use a dry cloth to remove excess polish. The surface should now have a shiny, mirror finish.

ステップ 6: Post-Sanding Cleaning

Even small bits of plastic dust can ruin post-processing (like painting), so thorough cleaning is a must.

  1. Blow away loose dust: Use an air blower or compressed air (on low pressure) to remove dust from crevices.
  2. Wipe with soap and water: Mix a small amount of mild soap (like dish soap) with warm water. Use a soft cloth to wipe the entire surface—this removes leftover dust and oil from your fingers.
  3. Dry completely: Pat the prototype with a lint-free towel, then let it air-dry for 15–30 minutes. Make sure no moisture remains before moving to coating or painting.

ステップ 7: Final Inspection

Before finishing, check that every part of the prototype is sanded correctly.

  1. Check for missed spots: Hold the prototype up to light—light will highlight any un-sanded areas or scratches.
  2. Verify size accuracy: Use a caliper to measure key dimensions. Over-sanding can reduce size, so make sure it still matches your design specs (許容範囲: ±0.1mm is ideal for most prototypes).
  3. Test surface smoothness: Run your finger over all edges and surfaces. If everything feels smooth and even, you’re done!

ステップ 8: Coating Protection (Optional: For Durability)

To make your sanded CNC plastic prototype more resistant to scratches, 化学物質, or UV light, add a coating.

  1. Choose a coating: プラスチック用, acrylic clear coat (スプレーオン) is best—it’s easy to apply and dries quickly.
  2. Apply thin layers: Spray 2–3 thin coats (wait 10–15 minutes between coats) instead of one thick coat. 厚いコートバブルまたはドリップ.
  3. Cure the coating: Let the prototype dry for 24 hours at room temperature. Avoid touching it during this time—fingerprints will be permanent.

Key Safety Tips for CNC Plastic Prototype Sanding

Sanding plastic creates fine dust that can be harmful if inhaled. Follow these safety rules to protect yourself:

  • Wear a dust mask: Use a N95 mask to filter out plastic dust—long-term exposure can irritate your lungs.
  • Work in a ventilated area: Open windows or use a fan to circulate air. If possible, use a dust collector (attached to electric tools) to capture dust as you sand.
  • Wear gloves: Disposable nitrile gloves prevent oil from your fingers transferring to the prototype (oil ruins sanding and coating) and protect your hands from rough sandpaper.
  • Avoid over-sanding thin parts: Thin plastic (less than 1mm thick) can warp or break if you press too hard. Use manual sanding with light pressure for these parts.

Yigu Technology’s Perspective on CNC Plastic Prototype Sanding

Yiguテクノロジーで, we see sanding as the “finishing touch” that makes CNC plastic prototypes stand out. Our team optimizes sanding by: 1) Using progressive grit sequences (80→240→600→1000) to ensure zero scratches; 2) Matching tools to part size—electric sanders for large panels, manual sanding for tiny details; 3) Adding a proprietary clear coat after sanding that boosts scratch resistance by 40%. ほとんどのCNCプラスチックプロトタイプの場合, we complete sanding (including polishing) in 2–4 hours, balancing speed with precision. We also train our team to check size accuracy during sanding, so prototypes always meet design specs.

よくある質問:

1. Do I need different sanding methods for different plastic materials (例えば。, ABS vs. PMMA)?

はい, but the difference is small. ABSプラスチック (softer) can be sanded with slightly less pressure—use 120-grit (not 80-grit) for initial sanding to avoid over-sanding. PMMA (アクリル) (harder) needs finer grits earlier—start with 120-grit and move to 400-grit faster, as it scratches less easily. For both, always use water-based sanding (damp sandpaper) if you want to reduce dust and get a smoother finish.

2. How do I fix over-sanding (例えば。, a small dip in the surface)?

If the dip is minor (less than 0.1mm), you can fix it with plastic filler (like Bondo Plastic Bumper Filler). Apply a tiny amount, let it dry (30 分), then sand it smooth with 400–600 grit sandpaper. For deeper dips, you may need to re-machine the part—this is why it’s better to sand slowly and check progress often!

3. Can I skip sanding if my CNC plastic prototype looks smooth?

Even if it looks smooth, CNC machining leaves micro-tool marks (too small to see but feelable). Skipping sanding will cause problems later: paint will peel, coatings won’t stick, or the prototype won’t fit with other parts. Spend 30–60 minutes sanding—it’s worth it for a high-quality result!

上にスクロールします