Silicone molding is a manufacturing process that transforms liquid or semi-solid silicone raw materials into elastomeric products with specific shapes and properties. Serve come spina dorsale per produrre tutto, dalle necessità quotidiane (per esempio., utensili da cucina) alle parti industriali di alta precisione (per esempio., sigilli). Ma con molteplici tecniche di stampaggio disponibili, how do you choose the right one for your project, and what key factors ensure success?
1. A Comparison of 6 Core Silicone Molding Methods
Different silicone molding techniques are designed for specific scenarios—from mass production to small-batch customization. The table below breaks down their core features, applicazioni, and key controls:
| Molding Method | Caratteristiche principali | Typical Applications | Critical Control Parameters |
| Stampaggio a compressione | Alta precisione; suitable for complex structures; produzione di massa | High-precision seals, guarnizioni automobilistiche | Temperatura dello stampo (160–200°C), pressione (5–50MPa), vulcanization time |
| Stampaggio ad iniezione | Alta efficienza; low scrap rate; automatizzato | Miniaturized parts (per esempio., electronic buttons, conductive connectors) | Velocità di iniezione (staged control), mold vacuum exhaust, plasticization temperature |
| Extrusion Molding | Continuous production; equal-section profiles | Pipes, sealing strips, rubber hoses | Die design, barrel segmented heating, laser diameter monitoring |
| Gate Molding | Flessibile; low-cost for small batches | Transparent crafts, mold prototypes, custom jewelry | Vacuum defoaming, layered infusion (for thick parts) |
| Rivestimento & Impregnation | Magro, uniform coverage; adheres to substrates | Fabric coating, PCB waterproof films, biomedical coatings | Coating thickness, adhesion (grid test), centrifugation speed (for impregnation) |
| Special Molding | Innovativo; solves complex needs | Cold runner: zero-waste parts; 3D printing-assisted: complex textures; Costampaggio: silicone + metal/plastic inserts | Isolamento (cold runner), resin type (3Stampa D), insert positioning (co-molding) |
2. Step-by-Step Guide to 3 Common Molding Processes
For beginners or those selecting a method, here’s a linear breakdown of three widely used workflows:
UN. Stampaggio a compressione (Ideal for High-Precision Seals)
- Preparazione del materiale: Weigh raw rubber, riempitivi, and vulcanizing agents per formula; mix evenly via a refiner.
- Plasticization: Reduce compound Mooney viscosity using the thin-pass method to improve plasticity.
- Preforming: Cut the compound into blanks that match the rough shape of the final product.
- Mold Vulcanization: Place blanks into the mold; heat and press in a flat vulcanizing machine (160–200°C, 5–50MPa).
- Post-trattamento: Trim excess material; conduct secondary vulcanization to remove volatiles and boost stability.
B. Stampaggio ad iniezione (Best for Miniaturized, Mass-Produced Parts)
- Alimentazione: Automatically feed granular or strip compound into the machine’s barrel.
- Plasticization: Heat the barrel to soften the compound (temperature varies by silicone type).
- Iniezione: Use high pressure to inject the softened compound into the closed mold cavity.
- Packing & Raffreddamento: Maintain pressure until the compound is initially cured; cool slightly to set shape.
- Sformatura: A manipulator automatically removes the finished product—no manual trimming needed for most designs.
C. Extrusion Molding (Great for Continuous Profiles)
- Progettazione di stampi: Customize the die opening to match the product’s cross-section (per esempio., round for pipes, rectangular for strips).
- Riscaldamento & Estrusione: Heat the barrel in segments (front: plasticization; middle: constant temperature; rear: formando); push compound through the die.
- Monitoraggio: Utilizzare un laser diameter gauge to real-time check product dimensions and adjust extrusion speed if needed.
- Traction & Taglio: Pull the extruded profile via a track system; cut it to the set length automatically.
3. Risoluzione dei problemi: Common Defects & Soluzioni
Even with proper process design, defects can occur. Below is a cause-and-effect guide to fix the most frequent issues:
| Defect Phenomenon | Root Cause | Practical Solution |
| Bubble Holes | Air trapped during mixing; gas released during vulcanization | Utilizzo vacuum defoaming before molding; adopt gradient heating for vulcanization (avoids sudden gas expansion) |
| Glue Shortage (Incomplete Filling) | Low silicone fluidity; insufficient glue injection volume | Increase injection pressure (for injection molding); optimize gate position to improve flow; preheat silicone slightly |
| Sticky Surface | Incomplete vulcanization; mold surface contamination | Extend vulcanization time or raise temperature; clean the mold with a solvent (per esempio., isopropyl alcohol) prima dell'uso |
| Dimensional Deviation | Uneven curing shrinkage; inconsistent mold temperature | Reserve a 1.5%–3% shrinkage allowance in mold design; ensure uniform mold heating (use temperature sensors) |
4. Materiale & Equipment Selection Guide
Choosing the right materials and equipment directly impacts product quality. Use this table to match your needs:
| Demand Scenario | Recommended Silicone Type | Supporting Equipment |
| Food-Grade Products (per esempio., silicone spatulas) | FDA-certified liquid silicone | Vacuum casting equipment (avoids contamination) |
| High-Precision Seals (per esempio., automotive oil seals) | Silicone with vapor-phase silica filler (boosts hardness) | Precision compression molding machine |
| Conductive Parts (per esempio., electronic buttons) | Precipitation-method conductive silicone rubber | Vertical injection machine + static elimination device |
| High-Temperature-Resistant Parts (per esempio., industrial pipes) | Phenyl silicone rubber (resists up to 300°C) | Extruder + laser diameter gauge |
5. Yigu Technology’s Perspective on Silicone Molding
Alla tecnologia Yigu, we see silicone molding as a driver of product innovation—not just a manufacturing step. For clients in healthcare, we’ve optimized coating molding to create biocompatible silicone films for medical devices, garantendo 99.8% adhesion and meeting global safety standards. Per i clienti del settore automobilistico, Nostro stampaggio a compressione process reduces seal defect rates to below 0.5% by refining temperature control and using high-purity fillers.
Looking forward, we’ll focus on two priorities: 1) Developing eco-friendly silicone materials that cut waste by 30% E 2) Integrating AI into stampaggio ad iniezione to real-time adjust parameters, boosting efficiency by 20%. We aim to make silicone molding more sustainable, preciso, and accessible for all industries.
Domande frequenti
- Which silicone molding method is best for small-batch custom products (per esempio., 50–100 unità)?
Gate molding is ideal—it’s low-cost, flessibile, and doesn’t require expensive molds. Use additive liquid silicone for high transparency (per esempio., custom crafts) and vacuum defoaming to ensure quality.
- How to ensure food-grade safety in silicone molding for kitchenware?
Primo, selezionare FDA-certified liquid silicone (no toxic additives). Secondo, use dedicated equipment (avoid cross-contamination with industrial-grade silicone). Terzo, conduct post-production tests (per esempio., leachate testing) to meet food safety standards.
- What’s the main difference between compression molding and injection molding for silicone parts?
Compression molding is better for complex, parti di alta precisione (per esempio., sigilli) but has longer cycle times. Injection molding is faster (ideal for mass production of mini parts like buttons) and has lower scrap rates, but requires higher initial mold investment.