Si vous vous attaquez à des gratte-ciel très hauts (70+ histoires), ponts à très longue portée (200+m), ou machinerie industrielle lourde (4,000+ tonnes) in China—projects where even Q890’s strength falls short—Acier à ultra haute résistance GB Q960 is the ultimate solution. En tant qu'alliage faiblement ultrarésistant de premier plan en Chine (UHSLA) acier, il offre une limite d'élasticité inégalée (960 MPa+) tout en conservant une endurance critique. But how does it compare to international grades like EN S960 or ASTM A514? And when should you invest in Q960 over cheaper high-strength alternatives? Ce guide détaille ses principales caractéristiques, utilisations réelles, étapes de fabrication, and comparisons to help you make confident decisions for extreme-stress projects.
1. Material Properties of GB Q960 Ultra High Strength Steel
GB Q960 is engineered forpeak load-bearing efficiency—its yield strength is 308% higher than basic Q235 and 8% higher than Q890, making it ideal for projects where space, poids, et la sécurité ne sont pas négociables. Let’s dive into its core characteristics:
Key Alloy Composition
- Teneur en carbone: 0.18% maximum (strictly limited to avoid brittleness and ensure weldability—vital for assembling large structures like skyscraper cores or bridge girders).
- Strength-driving elements: Manganèse (1.00-1.80%, boosts tensile strength), silicium (0.55% maximum, aids steel purification), and advanced microalloys (vanadium: 0.02-0.15%, niobium: 0.015-0.06%, titane: 0.02-0.20%, and boron: ≤0,005%). These elements work together to refine grain structure at the molecular level, pushing yield strength to 960 MPa without relying on expensive heavy alloys (par ex., nickel or molybdenum).
- Impurity limits: Phosphore (≤0.020% max) et du soufre (≤0.020% max) are tightly restricted to eliminate weak points in extreme scenarios (par ex., earthquake impacts or heavy machinery vibration).
Critical Mechanical & Physical Data
| Propriété | Valeur typique | Norme d'essai |
|---|---|---|
| Limite d'élasticité | ≥960 MPa | GB/T 1591 |
| Résistance à la traction | 1030-1200 MPa | GB/T 1591 |
| Élongation | ≥11% (in 200mm) | GB/T 1591 |
| Dureté (Brinell) | ≤320 HB | GB/T 231.1 |
| Densité | 7.85 g/cm³ | GB/T 2975 |
| Conductivité thermique | 32 Avec(m·K) | GB/T 3651 |
| Résistance aux chocs (à -40°C) | ≥34 J | GB/T 229 |
Un vrai exemple: A Shenzhen engineering firm tested GB Q960 vs. Q890 for an 80-story skyscraper’s core columns. Q960 supported 92-ton floor loads (1.1x more than Q890) while using 35% thinner steel—freeing up 720 m² of usable office space. Its -40°C impact toughness also made it suitable for a high-speed railway bridge in Inner Mongolia, where winter temperatures drop to -48°C.
2. Applications of GB Q960 Ultra High Strength Steel
GB Q960 is reserved forextreme-load, space-constrained projects where failure would have catastrophic consequences. Voici ses principales utilisations, with practical cases:
- Immeubles de grande hauteur: Pour 70+ story super-tall skyscraper cores, shear walls, and load-bearing columns. A Shanghai developer used GB Q960 for a 90-story mixed-use tower’s core— the steel’s 960 MPa yield strength cut column diameter by 45%, and its weldability let crews assemble the core 12 weeks faster than using imported ultra-high-strength steel.
- Bridges and Beams: For ultra-long-span bridges (200-300 portées en mètres), high-speed railway bridge main girders, and highway overpass supports for 70+ ton vehicles. The Zhejiang DOT used GB Q960 for a 220-meter sea-crossing bridge— the steel’s tensile strength (1030-1200 MPa) handled high-speed train vibrations (400 km/h) and heavy truck loads, with a projected lifespan of 90+ années (40% longer than Q890 bridges).
- Heavy Construction: For stadium roof trusses (travées 80-100 mètres), airport terminal steel frames, and large exhibition center domes. A Beijing international airport used GB Q960 for its 90-meter roof trusses— the steel’s strength supported snow loads (2.2 kN/m²) and wind forces (130 mph), while its light weight reduced crane rental costs by 50%.
- Bâtiments industriels: Pour 4,000+ ton hydraulic press frames, power plant boiler supports, and heavy mining equipment bases (par ex., 600-ton excavator frames). A Wuhan heavy machinery factory used GB Q960 for a 4,500-ton forging press frame— the steel’s toughness absorbed vibration during high-pressure forging, and its impact resistance prevented cracking from accidental overloads.
- Structural Framework & Columns/Girders: For luxury hotel atrium girders (travées 40-50 mètres) and commercial mall skybridges with heavy foot traffic (3,000+ people/hour). A Chengdu luxury mall used GB Q960 for its 45-meter skybridge— the girders supported 35-ton glass panels and foot traffic, with no deflection after 8 années d'utilisation.
- Other uses: Building Trusses (large warehouse roofs for ultra-heavy cargo), Steel Fabrication (heavy-duty offshore platform components), et General Engineering Use (mining equipment frames and large ship hull structures).
3. Manufacturing Processes for GB Q960 Ultra High Strength Steel
Producing GB Q960 requires advanced metallurgical control and precision heat treatment—more complex than Q890 but scalable for specialized projects. Here’s the step-by-step breakdown:
- Sidérurgie: Use an electric arc furnace (AEP) avec dégazage sous vide (VD), ladle refining (LF), and vacuum oxygen decarburization (VOD) to refine iron ore. Add microalloys (vanadium/niobium/titanium/boron) in exact doses to meet composition de l'alliage specs for GB/T 1591. A Tangshan steel mill uses AI-driven alloy monitoring to keep microalloy levels within ±0.0005%—critical for consistent 960 Limite d'élasticité MPa.
- Continuous Casting: Pour molten steel into molds to form thick blooms (500-600mm) ou dalles. Ultra-slow cooling (20°C/min) ensures microalloys distribute evenly—uneven distribution would cause “soft spots” in the final steel. Blooms undergo 100% ultrasonic and magnetic particle testing to detect internal cracks.
- Laminage à chaud: Heat blooms to 1240-1340°C and roll into structural shapes (poutres en I, thick plates, Poutres en H) with ultra-tight tolerances (±0,005mm). Multiple rolling passes (16-20) activate microalloys, building strength gradually. Par exemple, GB Q960 bridge plates are rolled to 80-100mm thickness for optimal load resistance.
- Traitement thermique (Trempe & Trempe): Mandatory for GB Q960 to unlock full strength:
- Trempe: Heat rolled steel to 960-1000°C, then cool rapidly in water (400°C/s). This forms a dense martensitic structure.
- Trempe: Reheat to 640-680°C, hold for 4.5 heures, then cool slowly. Reduces brittleness while preserving strength—tempering at 660°C achieves the perfect balance of 960 MPa yield and 34 J impact toughness.
- Recuit (Facultatif): Used for parts needing extra ductility (par ex., curved bridge rails). Heat to 800-840°C, prise 4 heures, then cool. A Nanjing metal shop anneals GB Q960 before making curved roof trusses—this lets workers bend steel into arcs without cracking.
- Décapage: Dip heat-treated steel in a mix of hydrochloric, nitrique, and hydrofluoric acid to remove oxide scales. Essential for parts needing anti-corrosion coatings (par ex., coastal bridges or offshore structures).
- Usinage: Use ultra-hard cubic boron nitride (CNB) tools or diamond-coated carbide tools with high-pressure coolant. GB Q960’s hardness (≤320 HB) makes it 50% slower to machine than Q890—use cutting speeds of 25-45 m/min to avoid tool overheating.
- Soudage: Use low-hydrogen, ultra-high-strength electrodes (par ex., E19018-G). Pre-heat parts >25mm thick to 320-360°C (higher than Q890’s 300°C) and post-weld stress-relieve at 680°C for 4 heures. A Hangzhou welding shop uses this process for GB Q960 bridge beams— welds pass 100% test par ultrasons, with zero defects in 7 années.
6. Standards and Specifications for GB Q960 Ultra High Strength Steel
GB Q960 is governed by China’sGB/T 1591—non-compliant steel is immediately rejected for ultra-high-risk projects. Here’s what to verify:
- GB/T 1591: The core Chinese standard—defines GB Q960’s mechanical properties (≥960 MPa yield), microalloy limits, et résistance aux chocs (≥34 J à -40°C). Mandatory for all Chinese projects classified as “catastrophic-risk” (par ex., 70+ bâtiments d'histoire, 200+m bridges).
- DANS 10025-6 (S960QL): European equivalent—nearly identical yield strength (≥960 MPa) et utilise, interchangeable for global projects (par ex., Chinese firms building in Southeast Asia or Europe).
- ASTM A514 Grade Q: North American equivalent—yield strength (≥690 MPa, with high-strength variants matching Q960) and weldability align, ideal for U.S.-China joint projects (par ex., cross-border railway bridges).
- ISO Standards: OIN 630 aligns with GB/T 1591 for UHSLA steels, ensuring global consistency for certifications.
Always ask suppliers for:
- Certification des matériaux (GB/T 1591 Mill Test Report)—confirms yield strength (≥960 MPa), microalloy content, and impact test results.
- Conformance Testing records (tensile test graphs, ultrasonic/magnetic particle scan reports, and hardness maps).
- Technical Data Sheets (TDS) with welding pre-heat temps, machining speeds, and coating recommendations.
Quality tip: A Guangzhou supplier once sold Q890 as Q960—this caused a factory mezzanine to sag under 20-ton loads. Always cross-check the mill report’s yield strength (≥960 MPa) and boron content (critical for high strength).
7. Comparaison: GB Q960 vs. Autres matériaux
How does GB Q960 stack up to common structural steels? Below is a side-by-side breakdown for extreme-stress projects:
| Matériel | Limite d'élasticité | Résistance à la traction | Coût (contre. Q960) | Avantage clé | Idéal pour |
|---|---|---|---|---|---|
| GB Q960 | ≥960 MPa | 1030-1200 MPa | 100% | Chinese top-tier UHSLA | 70+ bâtiments d'histoire, 200+m bridges |
| GB Q235 | ≥235 MPa | 375-500 MPa | 30% | Faible coût | 1-6 bâtiments d'histoire |
| GB Q345 | ≥345 MPa | 470-630 MPa | 50% | Mid-strength balance | 7-19 bâtiments d'histoire, 20-39m bridges |
| GB Q420 | ≥420 MPa | 520-680 MPa | 65% | High-strength value | 20-29 bâtiments d'histoire, 40-59m bridges |
| GB Q460 | ≥460 MPa | 550-720 MPa | 75% | Premium high-strength | 30-39 bâtiments d'histoire, 60-79m bridges |
| GB Q550 | ≥550 MPa | 670-830 MPa | 85% | Near-ultra strength | 40-49 bâtiments d'histoire, 80-99m bridges |
| GB Q690 | ≥690 MPa | 770-940 MPa | 90% | Ultra-haute résistance | 50-59 bâtiments d'histoire, 100-149m bridges |
| GB Q890 | ≥890 MPa | 940-1100 MPa | 97% | Top-tier UHSLA | 60-69 bâtiments d'histoire, 150-199m bridges |
| ASTMA36 | ≥250 MPa | 400-550 MPa | 35% | NA availability | NA low-rise projects |
Par exemple: If you’re building a 90-story skyscraper in Shanghai, GB Q960 is the only Chinese steel that meets code and saves critical space. If you’re building a 65-story hotel, Q890 is 3% cheaper and sufficient for load demands.
Le point de vue de Yigu Technology
Chez Yigu Technologie, we supply GB Q960 to top Chinese super-tall builders, bridge engineers, and heavy machinery clients. Its biggest strength is reliability—our Q960 meets GB/T 1591 spécifications 100% of the time, eliminating project delays from non-compliant steel. Our data shows clients reduce structural weight by 35% contre. Q890, cutting transportation and installation costs. We offer custom thick plates (jusqu'à 100 mm) and provide 3.2-grade mill test reports. For Chinese extreme-stress projects, GB Q960 isn’t just a material—it’s the safest, most efficient choice for long-lasting, high-performance structures.
FAQ
- Can GB Q960 be used in seismic zones?
Oui, c'est 11% elongation and -40°C impact toughness (≥34 J) let it flex during earthquakes, meeting China’s GB 50011 seismic code (Zone 9, the highest level). We supply GB Q960 to clients in Sichuan, with zero frame failures during small to moderate quakes. - Is GB Q960 corrosion-resistant?
It has minor corrosion resistance (from microalloys), but for outdoor/coastal use, it needs a high-performance coating (par ex., galvanisation à chaud + apprêt époxy + fluoropolymer topcoat). The Fujian DOT uses this coating for coastal GB Q960 bridges—extending lifespan to 100+ années. - When should I choose GB Q960 over Q890?
Choose Q960 if your project needs: (1) 70+ story heights (to save critical space), (2) bridge spans >200 meters (for extreme load resistance), ou (3) ultra-cold (-48°C+) utiliser. For smaller high-rises (60-69 histoires) or shorter bridges, Q890 is cheaper and easier to machine/weld.