Si vous vous attaquez à des gratte-ciel très hauts (60+ histoires), ponts à très longue portée (150+m), ou machinerie industrielle lourde (3,000+ tonnes) in China—projects where even Q690’s strength isn’t enough—Acier à ultra haute résistance GB Q890 is the ultimate solution. En tant qu'alliage faiblement ultrarésistant de premier plan en Chine (UHSLA) acier, il offre une limite d'élasticité inégalée (890 MPa+) tout en conservant une endurance critique. But how does it compare to international grades like EN S960 or ASTM A514? And when should you invest in Q890 over cheaper high-strength alternatives? Ce guide détaille ses principales caractéristiques, utilisations réelles, étapes de fabrication, and comparisons to help you make confident decisions for extreme-stress projects.
1. Material Properties of GB Q890 Ultra High Strength Steel
GB Q890 is engineered forpeak load-bearing efficiency—its yield strength is 279% higher than basic Q235 and 29% higher than Q690, making it ideal for projects where space, poids, et la sécurité ne sont pas négociables. Let’s dive into its core characteristics:
Key Alloy Composition
- Carbon Content: 0.18% maximum (strictly limited to avoid brittleness and ensure weldability—vital for assembling large structures like skyscraper cores or bridge girders).
- Strength-driving elements: Manganese (1.00-1.80%, boosts tensile strength), silicium (0.55% maximum, aids steel purification), and advanced microalloys (vanadium: 0.02-0.15%, niobium: 0.015-0.06%, titane: 0.02-0.20%, and boron: ≤0.005%). These elements work together to refine grain structure at the molecular level, pushing yield strength to 890 MPa without relying on expensive heavy alloys (par ex., nickel or molybdenum).
- Impurity limits: Phosphorus (≤0.025% max) and sulfur (≤0.025% max) are tightly restricted to eliminate weak points in extreme scenarios (par ex., earthquake impacts or heavy machinery vibration).
Critical Mechanical & Physical Data
| Propriété | Valeur typique | Test Standard |
|---|---|---|
| Yield Strength | ≥890 MPa | GB/T 1591 |
| Résistance à la traction | 940-1100 MPa | GB/T 1591 |
| Élongation | ≥12% (in 200mm) | GB/T 1591 |
| Dureté (Brinell) | ≤300 HB | GB/T 231.1 |
| Densité | 7.85 g/cm³ | GB/T 2975 |
| Conductivité thermique | 34 W/(m·K) | GB/T 3651 |
| Impact Toughness (at -40°C) | ≥34 J | GB/T 229 |
A real example: A Shanghai engineering firm tested GB Q890 vs. Q690 for a 70-story skyscraper’s core columns. Q890 supported 85-ton floor loads (1.3x more than Q690) while using 32% thinner steel—freeing up 650 m² of usable office space. Its -40°C impact toughness also made it suitable for a high-speed railway bridge in Heilongjiang, where winter temperatures drop to -45°C.
2. Applications of GB Q890 Ultra High Strength Steel
GB Q890 is reserved forextreme-load, space-constrained projects where failure would have catastrophic consequences. Here are its top uses, with practical cases:
- High-Rise Buildings: Pour 60+ story super-tall skyscraper cores, shear walls, and load-bearing columns. A Shenzhen developer used GB Q890 for an 80-story mixed-use tower’s core— the steel’s 890 MPa yield strength cut column diameter by 40%, and its weldability let crews assemble the core 10 weeks faster than using imported ultra-high-strength steel.
- Bridges and Beams: For ultra-long-span bridges (150-250 meter spans), high-speed railway bridge main girders, and highway overpass supports for 60+ ton vehicles. The Guangdong DOT used GB Q890 for a 180-meter sea-crossing bridge— the steel’s tensile strength (940-1100 MPa) handled high-speed train vibrations (350 km/h) and heavy truck loads, with a projected lifespan of 80+ années (35% longer than Q690 bridges).
- Heavy Construction: For stadium roof trusses (travées 70-90 mètres), airport terminal steel frames, and large exhibition center domes. A Beijing international airport used GB Q890 for its 80-meter roof trusses— the steel’s strength supported snow loads (2.0 kN/m²) and wind forces (120 mph), while its light weight reduced crane rental costs by 45%.
- Industrial Buildings: Pour 3,000+ ton hydraulic press frames, power plant boiler supports, and heavy mining equipment bases (par ex., 500-ton excavator frames). A Wuhan heavy machinery factory used GB Q890 for a 3,500-ton forging press frame— the steel’s toughness absorbed vibration during high-pressure forging, and its impact resistance prevented cracking from accidental overloads.
- Structural Framework & Columns/Girders: For luxury hotel atrium girders (travées 35-45 mètres) and commercial mall skybridges with heavy foot traffic (2,500+ people/hour). A Chengdu luxury mall used GB Q890 for its 40-meter skybridge— the girders supported 30-ton glass panels and foot traffic, with no deflection after 7 années d'utilisation.
- Other uses: Building Trusses (large warehouse roofs for ultra-heavy cargo), Steel Fabrication (heavy-duty offshore platform components), et General Engineering Use (mining equipment frames and large ship hull structures).
3. Manufacturing Processes for GB Q890 Ultra High Strength Steel
Producing GB Q890 requires advanced metallurgical control and precision heat treatment—more complex than Q690 but scalable for specialized projects. Here’s the step-by-step breakdown:
- Steelmaking: Use an electric arc furnace (EAF) with vacuum degassing (VD), ladle refining (LF), and vacuum oxygen decarburization (VOD) to refine iron ore. Add microalloys (vanadium/niobium/titanium/boron) in exact doses to meet composition de l'alliage specs for GB/T 1591. A Tangshan steel mill uses AI-driven alloy monitoring to keep microalloy levels within ±0.001%—critical for consistent 890 Limite d'élasticité MPa.
- Continuous Casting: Pour molten steel into molds to form thick blooms (450-550mm) or slabs. Ultra-slow cooling (25°C/min) ensures microalloys distribute evenly—uneven distribution would cause “soft spots” in the final steel. Blooms undergo 100% ultrasonic and magnetic particle testing to detect internal cracks.
- Hot Rolling: Heat blooms to 1230-1330°C and roll into structural shapes (I-beams, thick plates, H-beams) with ultra-tight tolerances (±0,01mm). Multiple rolling passes (14-18) activate microalloys, building strength gradually. Par exemple, GB Q890 bridge plates are rolled to 70-90mm thickness for optimal load resistance.
- Traitement thermique (Trempe & Tempering): Mandatory for GB Q890 to unlock full strength:
- Trempe: Heat rolled steel to 950-990°C, then cool rapidly in water (350°C/s). This forms a dense martensitic structure.
- Tempering: Reheat to 630-670°C, hold for 4 heures, then cool slowly. Reduces brittleness while preserving strength—tempering at 650°C achieves the perfect balance of 890 MPa yield and 34 J impact toughness.
- Recuit (Facultatif): Used for parts needing extra ductility (par ex., curved bridge rails). Heat to 780-820°C, prise 3.5 heures, then cool. A Nanjing metal shop anneals GB Q890 before making curved roof trusses—this lets workers bend steel into arcs without cracking.
- Pickling: Dip heat-treated steel in a mix of hydrochloric, nitric, and hydrofluoric acid to remove oxide scales. Essential for parts needing anti-corrosion coatings (par ex., coastal bridges or offshore structures).
- Usinage: Use ultra-hard cubic boron nitride (CNB) tools or diamond-coated carbide tools with high-pressure coolant. GB Q890’s hardness (≤300 HB) makes it 45% slower to machine than Q690—use cutting speeds of 30-50 m/min to avoid tool overheating.
- Soudage: Use low-hydrogen, ultra-high-strength electrodes (par ex., E17018-G). Pre-heat parts >25mm thick to 300-340°C (higher than Q690’s 280°C) and post-weld stress-relieve at 670°C for 3.5 heures. A Hangzhou welding shop uses this process for GB Q890 bridge beams— welds pass 100% ultrasonic testing, with zero defects in 6 années.
6. Standards and Specifications for GB Q890 Ultra High Strength Steel
GB Q890 is governed by China’sGB/T 1591—non-compliant steel is immediately rejected for ultra-high-risk projects. Here’s what to verify:
- GB/T 1591: The core Chinese standard—defines GB Q890’s mechanical properties (≥890 MPa yield), microalloy limits, and impact toughness (≥34 J at -40°C). Mandatory for all Chinese projects classified as “catastrophic-risk” (par ex., 60+ bâtiments d'histoire, 150+m bridges).
- DANS 10025-6 (S960QL): European equivalent—slightly higher yield strength (≥960 MPa) but similar uses, interchangeable for global projects (par ex., Chinese firms building in Southeast Asia or Europe).
- ASTM A514 Grade Q: North American equivalent—yield strength (≥690 MPa, with high-strength variants matching Q890) and weldability align, ideal for U.S.-China joint projects (par ex., cross-border railway bridges).
- ISO Standards: OIN 630 aligns with GB/T 1591 for UHSLA steels, ensuring global consistency for certifications.
Always ask suppliers for:
- Certification des matériaux (GB/T 1591 Mill Test Report)—confirms yield strength (≥890 MPa), microalloy content, and impact test results.
- Conformance Testing records (tensile test graphs, ultrasonic/magnetic particle scan reports, and hardness maps).
- Technical Data Sheets (TDS) with welding pre-heat temps, machining speeds, and coating recommendations.
Quality tip: A Guangzhou supplier once sold Q690 as Q890—this caused a factory mezzanine to sag under 18-ton loads. Always cross-check the mill report’s yield strength (≥890 MPa) and boron content (critical for high strength).
7. Comparaison: GB Q890 vs. Other Materials
How does GB Q890 stack up to common structural steels? Below is a side-by-side breakdown for extreme-stress projects:
| Matériel | Yield Strength | Résistance à la traction | Coût (contre. Q890) | Avantage clé | Idéal pour |
|---|---|---|---|---|---|
| GB Q890 | ≥890 MPa | 940-1100 MPa | 100% | Chinese top-tier UHSLA | 60+ bâtiments d'histoire, 150+m bridges |
| GB Q235 | ≥235 MPa | 375-500 MPa | 35% | Faible coût | 1-6 bâtiments d'histoire |
| GB Q345 | ≥345 MPa | 470-630 MPa | 55% | Mid-strength balance | 7-19 bâtiments d'histoire, 20-39m bridges |
| GB Q420 | ≥420 MPa | 520-680 MPa | 70% | High-strength value | 20-29 bâtiments d'histoire, 40-59m bridges |
| GB Q460 | ≥460 MPa | 550-720 MPa | 80% | Premium high-strength | 30-39 bâtiments d'histoire, 60-79m bridges |
| GB Q550 | ≥550 MPa | 670-830 MPa | 90% | Near-ultra strength | 40-49 bâtiments d'histoire, 80-99m bridges |
| GB Q690 | ≥690 MPa | 770-940 MPa | 95% | Ultra-haute résistance | 50-59 bâtiments d'histoire, 100-149m bridges |
| ASTM A36 | ≥250 MPa | 400-550 MPa | 40% | NA availability | NA low-rise projects |
Par exemple: If you’re building an 80-story skyscraper in Shenzhen, GB Q890 is the only Chinese steel that meets code and saves critical space. If you’re building a 55-story hotel, Q690 is 5% cheaper and sufficient for load demands.
Yigu Technology’s Perspective
Chez Yigu Technologie, we supply GB Q890 to top Chinese super-tall builders, bridge engineers, and heavy machinery clients. Its biggest strength is reliability—our Q890 meets GB/T 1591 specs 100% of the time, eliminating project delays from non-compliant steel. Our data shows clients reduce structural weight by 32% contre. Q690, cutting transportation and installation costs. We offer custom thick plates (up to 90mm) and provide 3.2-grade mill test reports. For Chinese extreme-stress projects, GB Q890 isn’t just a material—it’s the safest, most efficient choice for long-lasting, high-performance structures.
FAQ
- Can GB Q890 be used in seismic zones?
Yes—its 12% elongation and -40°C impact toughness (≥34 J) let it flex during earthquakes, meeting China’s GB 50011 seismic code (Zone 9, the highest level). We supply GB Q890 to clients in Sichuan, with zero frame failures during small to moderate quakes. - Is GB Q890 corrosion-resistant?
It has minor corrosion resistance (from microalloys), but for outdoor/coastal use, it needs a high-performance coating (par ex., hot-dip galvanizing + epoxy primer + fluoropolymer topcoat). The Fujian DOT uses this coating for coastal GB Q890 bridges—extending lifespan to 90+ années. - When should I choose GB Q890 over Q690?
Choose Q890 if your project needs: (1) 60+ story heights (to save critical space), (2) bridge spans >150 meters (for extreme load resistance), ou (3) ultra-cold (-45°C+) utiliser. For smaller high-rises (50-59 histoires) or shorter bridges, Q690 is cheaper and easier to machine/weld.