Steel Raised Expanded Metal: A Guide to Products, Usos & Propiedades

metal parts custom manufacturing

If you’re looking for a strong, versatile metal mesh that offers grip, airflow, y durabilidad, steel raised expanded metal is an excellent choice. Unlike flattened expanded metal, it has raised strands that create texture—perfect for walkways, security fences, or architectural accents. This guide covers everything you need to know to choose, usar, and install this practical material. […]

If you’re looking for a strong, versatile metal mesh that offers grip, airflow, y durabilidad, steel raised expanded metal is an excellent choice. Unlike flattened expanded metal, it has raised strands that create texture—perfect for walkways, security fences, or architectural accents. This guide covers everything you need to know to choose, usar, and install this practical material.

1. Steel Raised Expanded Metal – Product Fundamentals

Steel raised expanded metal (también llamadoraised mesh oraised steel grating) is made from a single steel sheet, giving it more strength than welded or woven mesh. It’s defined by its raised, diamond-shaped strands that form a textured surface. Here are the most common product forms:

Product TypeKey FeaturesUsos comunes
Raised expanded metal sheetFlat, cut-to-size sheets (p.ej., 4ft×8ft)Walkways, guardias de la máquina, shelf bottoms
Raised expanded metal panelLarger, pre-assembled panels (for facades)Architectural cladding, sunshade screens
Raised expanded metal rollContinuous lengths (1–3m width)Large-scale projects (p.ej., warehouse fences)
Raised steel grateThick strands (for heavy loads)Trench covers, trailer ramps
Raised metal latticeSmall openings (for fine filtering)HVAC filters, particiones decorativas

Real Example: A construction company usedraised expanded metal sheet to make temporary walkways on a building site. The raised strands prevented workers from slipping in rain, and the mesh’s strength supported tool carts—saving the company from 2 potential slip-and-fall incidents.

2. Fabricación & Production Processes

Steel raised expanded metal is made in a few key steps that turn a solid steel sheet into a textured mesh:

  1. Steel Coil Feeding: Primero, a steel coil feeding system feeds a solid steel coil (cold-rolled or hot-rolled) into the expansion machine.
  2. corte & Stretching: The machine uses sharp dies to cut slits in the steel sheet (this isdie cutting steel mesh). Entonces, rollers stretch the sheet to create diamond-shaped openings—this step forms the “raised” strands. Unlike flattened mesh, it skips the cold-roll flattening step.
  3. Pattern Design: Elraised pattern die design determines the opening size (p.ej., small diamonds for filters, large diamonds for walkways).
  4. Line Speed ControlExpanded metal line speed is adjusted to ensure consistent openings—too fast, and the mesh can tear; demasiado lento, and production is inefficient.
  5. Control de calidad: Every batch is checked against standards likeASTM F1267 steel expanded metal yISO 9001 steel mesh to ensure strength and opening accuracy. Many factories also followISO 14001 for eco-friendly production.

Fun Fact: The “slit-and-stretch process” doesn’t waste steel—since it’s made from a single sheet, there’s no scrap (unlike woven mesh, which cuts wire into small pieces).

3. Material Specifications & Estándares

To pick the right raised expanded metal, you need to know its material type and key specs. Here’s what matters:

Materiales comunes

Tipo de materialKey TraitsMejor para
Carbon steel raised expanded metalAsequible, fuerte (ASTM A36)Indoor walkways, guardias de la máquina
Galvanized steel raised meshresistente al óxido (ASTM A123 coating)Outdoor fences, trailer ramps
Stainless steel raised expanded metalCorrosion-proof (SUS304/SUS316)Food processing, marine projects

Especificaciones clave

  • Strand Thickness: Typically 1.5mm–10mm (thicker = stronger; 4mm–6mm is best for walkways).
  • SWD/LWDSWD (Short Way of Diamond) (p.ej., 25milímetros) yLWD (Long Way of Diamond) (p.ej., 50milímetros) describe opening size.
  • FortalezaTensile strength raised mesh ranges from 400–600 MPayield strength steel mesh is 250–400 MPa (stronger than woven mesh).

4. Dimensions, Patterns & Open-Area Configurations

The size and pattern of raised expanded metal determine its use. Here are common options:

Pattern/SizeOpen-Area PercentageUsos
1/2 pulgada #13 raised expanded steel~60%HVAC filters, small machine guards
3/4 pulgada #9 raised mesh~50%Shelf bottoms, decorative screens
1 pulgada #13 raised metal~65%Walkways, catwalks
1-1/2 pulgada #16 raised steel~70%Facade cladding, sombrillas
Micro mesh raised steel<30% (small openings)Fine filtering (p.ej., oil filters)

Open-Area Tip

Higher open-area percentage (p.ej., 70%) means more airflow/light—great for facades. Lower percentage (p.ej., 30%) is better for filtering or security (harder to climb through).

5. Acabados superficiales & Recubrimientos

To boost durability and appearance, raised expanded metal can have different finishes:

  • Hot-Dip Galvanized: The mesh is dipped in molten zinc—best for outdoor use (resists rust for 10+ años).
  • Electro-Galvanized: A thin zinc layer applied via electricity—cheaper than hot-dip, good for indoor/outdoor with light moisture.
  • Powder Coated: A dry powder baked on (polyester or epoxy)—comes in colors (negro, gray) and resists scratches (ideal for architectural projects).
  • PVC Coated: A soft PVC layer—adds grip (great for flooring) and resists chemicals (used in food plants).
  • Mill Finish: No coating—natural steel look, best for indoor, dry areas (p.ej., shelf mesh).

Ejemplo: A coastal restaurant usedstainless steel raised expanded metal with a marine-grade coating for its outdoor patio screens. The coating resists saltwater rust, and the mesh lets ocean breezes through.

6. Mecánico & Physical Properties

Steel raised expanded metal’s strength and performance make it stand out:

PropiedadTypical Values (Acero carbono)Why It Matters
Resistencia a la tracción450–550 MPaSupports heavy loads (p.ej., tool carts on walkways)
Load Capacity300–800 lbs/sq ft (depends on strand thickness)Safe for pedestrian traffic
Resistencia al impactoResiste 15 J of force (no cracking)Doesn’t break if hit by tools or debris
Slip ResistanceAlto (textured raised strands)Prevents falls on wet walkways
Weight per m²5–20 kg/m²Easy to install (lighter than solid steel)

Test Result: A lab test showed that 6mm strand raised mesh withstood 500 lbs/sq ft—enough for 2 workers plus tools.

7. Aplicaciones & End-Use Industries

Steel raised expanded metal is used across industries for its versatility:

  • ConstrucciónRaised steel mesh catwalkstrench covers, ypeldaños de escalera (seguro, slip-resistant).
  • SeguridadSteel mesh security fences and machine guards (hard to climb/cut through).
  • ArquitecturaRaised steel mesh façade cladding and sunshades (modern look, lets light through).
  • IndustrialHVAC expanded steel filtersconveyor belt steel mesh, and mining screens (durable, fácil de limpiar).
  • AutomotorRadiator grille and trailer ramps (resists road debris).

Estudio de caso: A solar farm usedgalvanized raised expanded metal for its panel supports. The mesh let wind pass through (reducing wind damage) and withstood outdoor weather for 5 years without rust.

8. Installation, Fastening & Accesorios

Installing raised expanded metal is easy with the right tools and accessories:

  • sujetadores: Usarself-drilling screws (for wood/steel frames) ograting clamps (for metal walkways). For outdoor projects, choose corrosion-resistant fasteners.
  • Edging: Addangle iron edging raised mesh oU-edge trim to prevent sharp edges (safer for installation).
  • Framing: Usarsteel expanded metal framing (galvanized or powder-coated) to support large panels (p.ej., facades).
  • Suspension: For ceilings or overhead screens, usarsuspension rods to hang the mesh securely.

Installation Tip: Leave a 10mm gap between mesh sheets to allow for thermal expansion (prevents warping in hot weather).

La perspectiva de la tecnología Yigu

En Yigu Tecnología, recomendamossteel raised expanded metal for clients needing strength and texture. We supply custom-cut mesh—fromSUS316 stainless steel for marine projects to galvanized carbon steel for outdoor fences. We also provide installation guides, helping clients choose the right fasteners and edging. Our mesh meets ASTM and ISO standards, ensuring durability—we’ve helped construction and security clients cut maintenance costs by 30% vs. woven mesh.

Preguntas frecuentes

  1. Is steel raised expanded metal more slip-resistant than flattened mesh?
    Sí! The raised strands create texture that grips shoes, making it better for wet walkways or ramps. Flattened mesh has a smooth surface, which can be slippery when wet.
  2. Can it be used for outdoor projects?
    Absolutely—choose galvanized or stainless steel with a marine-grade coating. This resists rust from rain/saltwater, lasting 10+ años al aire libre.
  3. How do I clean raised expanded metal?
    For most dirt, hose it down with water. For grease (p.ej., in kitchens), use a mild detergent and a brush (the raised strands are easy to scrub). Avoid harsh chemicals—they can damage coatings.